Re-based Diffusion Barrier on a Ni-based Superalloy: Its Formation, Macro- and Micro-structures, and Thermal Stability - Yongming Wang - Libros - Scholars' Press - 9783639761023 - 6 de enero de 2015
En caso de que portada y título no coincidan, el título será el correcto

Re-based Diffusion Barrier on a Ni-based Superalloy: Its Formation, Macro- and Micro-structures, and Thermal Stability

Precio
€ 166,49

Pedido desde almacén remoto

Entrega prevista 8 - 16 de dic.
Los regalos de Navidad se podrán canjear hasta el 31 de enero
Recibe notificaciones sobre nuevos lanzamientos de Yongming Wang
Añadir a tu lista de deseos de iMusic

Aún no valorado

The gas turbine doubtlessly is one of the most important modern machines to convert energy from heat to power, and improving its efficiency is a ceaseless task. The most practical route to increase the efficiency is to increase the maximum operating temperature. Over the past several decades, the improvement of this temperature was constantly attained by the developments of thermal barrier coating and superalloys, but almost reached a limit because the microstructural deterioration of both the base superalloy and the coating system due to the interdiffusion between them can be dramatically aggravated by further increasing temperature. The novel diffusion barrier type bond coat, therefore, is a solution to this issue. This book introduces how to form a rhenium-based diffusion barrier on a nickel-based superalloy. The formation process and thermal stability of the diffusion barrier are discussed through analyzing its macro- and micro-structures by XRD, EBSD, EPMA, SEM, and TEM, etc. This work provides the fundamental knowledge about the novel coating system, and should be especially useful to researchers and students in high-temperature materials science and technology.

Medios de comunicación Libros     Paperback Book   (Libro con tapa blanda y lomo encolado)
Publicado 6 de enero de 2015
ISBN13 9783639761023
Editores Scholars' Press
Páginas 204
Dimensiones 12 × 150 × 220 mm   ·   322 g
Lengua Alemán  

Mas por Yongming Wang